ASTM B168 UNS N06600 Plate

ASTM B168 UNS N06600 Plate


1. Standard: ASTM B168, ASME SB168
2. Width: 0~2500mm or as per your requirements
3. Length: 0~12m or as per your requirements
4. Thickness: 0.3~ 200mm or as per your requirements
Envoyez demande
Présentation du produit

Supplier Manufacturer of ASTM B168 UNS N06600 rolled Plate sheet and strip in China, Contact us to get price list, Sizes & Free Sample!

 

ASTM B168 UNS N06600 Plate is designed for use in high temperature ranges from cryogenic to 2000 degree F (1093 degree ). Inconel 600 Sheet is non-magnetic and easily weldable. Nickel 600 Plate has excellent resistance to chloride stress corrosion cracking as well as resistance to carburization or moderate temperature sulfur-containing environments.

 

Inconel 600 UNS N06600 Plate at the best price in China. We stock Alloy 600 plate in thicknesses from 3/16" (2.8mm) to 2" (50.8mm) for applications in chemical processing equipment, nuclear engineering, heat treating industries, heat exchangers, and more.

 

ASTM B168 UNS N06600 Plate Delivery Conditions:

  • Inconel 600 hot-rolled plate: annealed; or as-rolled
  • Inconel 600 hot-rolled sheet: annealed
  • Inconel 600 cold-rolled sheet: annealed; or hard
  • Inconel 600 cold-rolled strip: annealed; skin-hard
ASTM B168 UNS N06600 Plate

 

 

2.4816 Inconel 600 Plate Dimensions

2B – Cold rolled, heat treated, pickled, skin passed 0.25–8.0 max. 2032
2D – Cold rolled, heat treated, pickled 0.4–6.35 max. 1524
2E – Cold rolled, heat treated, mechanically descaled 0.4–8.0 max. 2032
2R – Cold rolled, bright annealed 0.25–3.5 max. 1524
2H – Work hardened 0.4–6.35 max. 1524
0.5–4.0 max. 1524

ASTM B168 UNS N06600 Cold Rolled Sheet Coil Supplier and Inconel 600 Hot Rolled Plate Manufacturer in China

 

B168M UNS N06600 sheet tolerance in width and length

Inconel 600 Plate Under 3/8 in. [9.52 mm] in Thickness 3/8[9.52] to 1/2[12.70 mm] in. incl in
Over 1/2[12.70 mm] to 1 in. [25.40 mm] in Thickness
Over 108[2743]   7/8 [22.22] 5/8[15.88] 1[25.40] 11/16[17.46] 1[25.40] 7/8[22.22]
Over 84[2134] to
108[2743] incl
  3/8 [9.52] 5/16[7.94] 7/16[11.11] 3/8[9.52] 9/16[14.29] 1/2[12.70]
Over 108[2743]   7/16 [11.11] 3/8[9.52] 1/2[12.70] 7/16[11.11] 11/16[17.46] 5/8[15.88]
Over 60[1524] to
84[2134] incl
over 144[3658] to
240[6096]
1/2 [12.70] 3/8[9.52] 11/16[17.46] 7/16[11.11] 3/4[19.05] 1/2[12.70]
48[1219] and under   3/8 [9.52] 3/16[4.76] 1/2[12.70] 1/4[6.35] 5/8[15.88] 5/16[7.94]
Over 48[1219] to
60[1524] incl
  7/16 [11.11] 1/4[6.35] 5/8[15.88] 5/16[7.94] 3/4[19.05] 3/8[9.52]
Over 84[2134] to
108[2743] incl
  9/16 [14.29] 7/16[11.11] 3/4[19.05] 1/2[12.70] 7/8[22.22] 5/8[15.88]
Over 48[1219] to
60[1524] incl
  5/8 [15.88] 5/16[7.94] 3/4[19.05] 3/8[9.52] 3/4[19.05] 1/2[12.70]
Over 108[2743]   5/8 [15.88] 1/2[12.70] 7/8[22.22] 5/8[15.88] 1[25.40] 11/16[17.46]
48[1219] and under   1/2 [12.70] 1/4[6.35] 5/8[15.88] 5/16[7.94] 3/4[19.05] 3/8[9.52]
Over 48[1219] to
60[1524] incl
  1/4 [6.35] 3/16[4.76] 5/16[7.94] 1/4[6.35] 7/16[11.11] 3/8[9.52]
Over 60[1524] to
84[2134] incl
over 240[6096] to
360[9144]
11/16 [17.46] 7/16[11.11] 3/4[19.05] 1/2[12.70] 7/8[22.22] 5/8[15.88]
48[1219] and under   3/16 [4.76] 1/8[3.18] 1/4[6.35] 3/16[4.76] 3/8[9.52] 5/16[7.94]
Over 60[1524] to
84[2134] incl
144[3658] and
5/16 [7.94] 1/4[6.35] 3/8[9.52] 5/16[7.94] 1/2[12.70] 7/16[11.11]
Over 84[2134] to
108[2743] incl
  3/4 [19.05] 9/16[14.29] 7/8[22.22] 5/8[15.88] 1[25.40] 3/4[19.05]

 

Q: About ASTM B168 UNS N06600 Plate Price per kg?

A: Prices from ranges $25.00 to $35.00 per kilogram, vary depending on size, wall thickness, supplier etc.

A: Delivery time is within 5-21 days

 

 

 

étiquette à chaud: astm b168 uns n06600, Alloy 600 Sheet, Alloy 600 plate, uns n06600, Inconel 600 suppliers